ASTM A573-05 Structural Carbon Steel Plates of Improved Toughness
Grade | Thickness | Chemical Compositions % | Tension Test | |||||||
C | Si | Mn | P | S |
Yield Point ksi (N/mm²) |
Tensile Strength ksi (N/mm²) |
Elongation | |||
Test piece in(mm) |
% min |
|||||||||
Gr.58 | t≤38.1 | 0.23 Max | 0.10-0.35 | 0.60-0.90 | 0.035 Max | 0.040 Max |
32(220) min |
58-71 (400-490) |
GL=8(200) GL=2(50) |
21 24 |
Gr.65 | t≤12.70 | 0.24 Max | 0.15-0.40 | 0.85-1.20 |
35(240) min |
65-77 (450-530) |
GL=8(200) GL=2(50) |
20 23 |
||
12.7<t≤38.10 | 0.26 Max | |||||||||
Gr.70 | t≤12.70 | 0.27 Max |
42(290) min |
70-90 (485-620) |
GL=8(200) GL=2(50) |
18 21 |
||||
12.70<t≤38.10 | 0.28 Max |
Remarks
1. For plates wider than 24 in.(600mm), the elongation requirement is reduced two percentage points. See elongation requirement adjustments in the Tension Tests Section of Specification A6/A6M.
2. The upper limit of manganese for Gr.58 may be exceeded, provided that the carbon content plus 1/6 manganese content does not exceed 0.40% based on heat analysis.
3. Gr.58,65 for each reduction of 0.01% below the specified carbon maximum, an increase of 0.06% manganese above the specified maximum is permitted, up to a maximum of 1.50% and 1.60% for Grades 70.